30% carbon fiber reinforcement, thermal stability, wear and friction improvement
15% carbon fiber reinforcement, thermal stability, wear and friction improvement
15% carbon fiber reinforcement, thermal stability, lubrication
30% fiberglass reinforcement, flame retardant, heat stable, heat resistance during hot welding and reflow process
40% fiberglass reinforcement, thermally stable
Thermal stability, reflectivity at 460nm: 95.5% (initial value) and 91.1% (160 ℃ for 8 hours)